NK CAST LC-13
Type of Product : Fire Clay Light Weight Castable
Physical Properties:
|
Raw material basis |
Light weight fire clay |
|
Max Service Temperature (°C) |
1300 |
|
Dry castable required (Kg/m3) |
1400 |
|
Approximate amount of water required (liters/40 Kg) |
11 – 13 |
|
Bulk density after drying at 110°C (Kg/m3) |
1500 |
|
Grain size (mm) |
0 – 5 |
|
Thermomechanical
Properties: |
Cold Crushing Strength (Kg/Cm2) |
Modulus of Rupture (Kg/Cm2) |
Linear Change (%) |
|
After drying at 110 ° C
|
≥ 55 |
≥ 12 |
-0.8 to -0.2 |
|
After heating at 1200° C |
≥ 40 |
≥ 10 |
– 0.8 to – 0.2 |
Thermal Conductivity (KCal/m.h.˚C):
|
@ 400˚C |
0.42 |
|
@ 600˚C |
0.45 |
|
@ 800˚C |
0.48 |
Chemical Analysis (%):
|
Al2O |
SiO2 |
Fe2O3 |
TiO2 |
CaO |
Na2O+K2O+LiO2 |
|
35 |
38 |
7 |
3 |
13 |
2.5 |
Packing in 40 Kg Bags.
– All data subject to reasonable deviations, and therefore, should not be used for specification purposes.
– ASTM Test Methods, where applicable, used for determination of data.