NK-CAST Al-SiC/48-10
Type of Product: High Alumina SiC Low Cement Dense Castable
Physical Properties:
Raw material basis | Silicon carbide and fire clay |
Max service temperature (°C) | 1500 |
Dry castable required (Kg/m3) | 2350 – 2450 |
Approximate amount of water required (%) | 7.5 – 8 |
Bulk density after drying at 110°C (Kg/m3) | 2400 – 2500 |
Grain size (mm) | 0 – 4 |
Thermomechanical
Properties: | Cold Crushing Strength (Kg/Cm2) | Modulus of Rupture (Kg/Cm2) | Linear Change (%) |
After Drying at 110 ° C | ≥ 700 | ≥ 75 | negligible |
After heating at 1400° C | ≥ 1000 | ≥ 95 | 0.5 to -1 |
Chemical Analysis (%):
SiC | Al2O3 | SiO2 | Fe2O3 | CaO |
8 – 11 | 45 – 50 | 32 – 38 | 1.5 – 2 | 4 – 4.5 |
Packing in 30 Kg Bags.
– All data subject to reasonable deviations, and therefore, should not be used for specification purposes.
– ASTM Test Methods, where applicable, used for determination of data.